Журналы →  Chernye Metally →  2022 →  №9 →  Назад

70 years of the Department of Metal Technology and Aviation Materials Science Samara National Research University named after S.P. Korolev
Название Influence of long-term thermal cycling in a corrosive environment on the change in properties and microstructure of SCh20 cast iron
DOI 10.17580/chm.2022.09.07
Автор K. K. Chaplygin, S. V. Voronin
Информация об авторе

Samara National Research University named after Academician S. P. Korolev, Samara Russia:

K. K. Chaplygin, Postgraduate Student, Dept. of Metal Technology and Aviation Materials Science, e-mail: chapkostya96@mail.ru
S. V. Voronin, Cand. Eng., Associate Prof., Dept. of Metal Technology and Aviation Materials Science

Реферат

The article considers the study of a metal sample of the wall of the working chamber of the compressor cylinder of the model 5G-100-7 made of SCh20 cast iron, which has been in operation since 1992 and is intended for pyrogas compression at a temperature of 110 °C, decommissioned due to the end of its service life. Mechanical tests were carried out as a result of which the mechanical characteristics of the metal were determined, such as tensile strength and Brinell hardness. The chemical composition of the metal was determined and an excess of sulfur content was established, which is explained by metal contamination due to the presence of sulfur compounds in the compressible medium. Pollution of the compressible medium is caused by the imperfection of the technology for cleaning pyrolysis gas from various impurities. The microstructure of the center of the wall and the edge of the sample, which are in direct contact with the compressible medium, has been studied. It has been established that the microstructure of the sample center is typical for gray cast iron. Along the edges of the wall, rounded corrosion pits and corrosion pits are observed. As a result of the analysis of the microstructure of the surface of the wall of the working chamber, it was found that there is a layer on the surface with dissolved graphite inclusions and the formation of pearlite grains with cementite along the boundaries. Under the surface layer, ferrite grains were found, as a result of the decomposition of perlite, and the transition of carbon to graphite with a morphology different from the base metal and cementite along the periphery of graphite inclusions and ferrite grains.

Ключевые слова Thermal cycling, mechanical testing, gray cast iron, compressor, pyrolysis gas, corrosion
Библиографический список

1. Tsybulko А. Е., Bakhtin D. Е. Evaluation of the strength of materials in the brittle and plastic state under complex loading. Vostochno-Evropeyskiy zhurnal peredovykh tekhnologiy. 2008. No. 2/4 (32). pp. 47–49.
2. Azarenkov N. А., Litovchenko S. V., Neklyudov I. М., Stoev P. I. Corrosion and protection of metals. Part 1. Chemical corrosion of metals: textbook. Kharkov, 2007. 187 p.
3. General technical conditions for the repair of reciprocating compressors. Volgograd, 1985. 361 p.
4. GOST 1497–84. Metals. Methods of tension test. Introduced: 01.01.1986.
5. GOST 9012–59. Metals. Method of Brinell hardness measurement. Introduced: 01.01.1960.
6. GOST 1412–85. Flake graphite iron for castings. Grades. Introduced: 01.01.1987.
7. Beschastnov М. V., Sokolov V. М. Prevention of accidents in chemical production. Moscow: Khimiya, 1979. 392 p.
8. Urinov А. А., Rakhmatov B. B. Analysis of the technological process for production of gas products in order to develop waste-free technologies. Molodoy ucheny. 2016. No. 3 (107). pp. 218–220.
9. Gulieva S. N., Azizlin N. R. Application of the process of pyrolysis and purification of natural gas from sulfur compounds. NAU. 2021. No. 73-3. pp. 31, 32.
10. Hsu Ch., Shy Yh., Yu Yh., Lee Sc. Effect of austempering heat treatment on fracture toughness of copper alloyed gray iron. Materials Chemistry and Physics. 2000. Vol. 63, Iss. 1. pp. 75–81.
11. Rajani B., Kleiner Y. External and internal corrosion of large-diameter cast iron mains. Journal of Infrastructure Systems. 2013. Vol. 19, Iss. 4. pp. 486–495.
12. Czajczyńska D., Krzyżyńska R., Jouhara H. Hydrogen sulfide removal from waste tire pyrolysis gas by inorganics. International Journal of Hydrogen Energy. 2022. Available at: https://www.sciencedirect.com/science/article/pii/S0360319922011193 (accessed: 01.05.2022 г.).
13. Dobrotvorskiy А. М., Gyulikhandanov Е. L., Maslikova Е. I. Destruction of pipelines made of low-carbon structural steels in a hydrogen sulfide-containing environment. Materialovedenie. Energetika. 2017. No. 2. pp. 159–164.
14. Liyanage K., Dhar A. S. Stresses in cast iron water mains subjected to non-uniform bedding and localised concentrated forces. International Journal of Geotechnical Engineering. 2018. Vol. 12, Iss. 4. pp. 368–376.
15. Berrekia H., Benzerga D., Haddi A. Behavior and damage of a pipe in the presence of a corrosion defect depth of 10% of its thickness and highlighting the weaknesses of the ASME/B31G method. Frattura ed Integrità Strutturale. 2019. Vol. 13, Iss. 49. pp. 643–654.
16. Cerit M., Genel K., Eksi S. Numerical investigation on stress concentration of corrosion pit. Engineering Failure Analysis. 2009. Vol. 16, Iss. 7. pp. 2467–2472.
17. Ji J., Zhang C., Kodikara J., Yang S.Q. Prediction of stress concentration factor of corrosion pits on buried pipes by least squares support vector machine. Engineering Failure Analysis. 2015. Vol. 55. pp. 131–138.
18. Fu G., Zhang C., Deo R., Rathnayaka S., Shannon B., Kodikara J. A model of stress concentration factors for external corrosion patches on large-diameter underground cast iron pipes. Sustainable and Resilient Infrastructure. 2020. Vol. 14. pp. 1–12.
19. Kovydin S. А., Abalikhina О. V. Computer study of the stress-strain state of pipes of superheaters made of 12Kh1MF steel of a high-pressure boiler. Gagarin Readings - 2019: Collection of abstracts. Moscow: MAI, 2019. Р. 961.

Language of full-text русский
Полный текст статьи Получить
Назад